| Basic Mechanical Testing | Scope |
| Tensile | RT |
| Tensile | Up to 1000 ℃ |
| Compression | RT |
| Compression | Up to 1000 ℃ |
| Hardness | Macro and Micro |
| Impact Testing | Charpy Notch Test |
| 3P and 4 P Bend Test |
| Fatigue | Scope |
| Low-cycle fatigue | LCF test up to 12 Hz |
| High Cycle fatigue | HCF test up to 70 Hz |
| Advanced Low-cycle fatigue | Constant amplitude, strain controlled up to 12 Hz, calculates and corrects for thermal expansion (1000 ℃) |
| Advanced high-cycle fatigue | HCF test up to 70 Hz, calculates and corrects for thermal expansion (1000 ℃) |
| Fracture Module | Scope |
| Fatigue crack growth rate | Paris curve (c,n) determination |
| K1C Fracture toughness | Linear elastic plain strain fracture toughness |
| J1C Fracture toughness | Determination of fracture toughness using K, J, and CTOD (δ). Toughness can be measured in the R-curve format. |
| Advanced Tests at High temperature | Scope |
| Stress rupture | Up to 1100 ℃ |
| Creep | Up to 1100 ℃ |